- Contact Person : Mr. Ke Lijun
- Company Name : Huangshan Hongya Chemical Co., Ltd.
- Tel : 86-559-7511965
- Fax : 86-559-7511802
- Address : Anhui,Huangshan,109 Hengjiang Road,Haiyang Town, Xiuning County,Huangshan, Anhui
- Country/Region : China
- Zip : 245400
HY-888 Silicone Oil for polyester three-Dimensional Crimp Fibre for Special Smoothness
HY-888 Silicone Oil for polyester three-Dimensional Crimp Fiber for Special Smoothness
This product is used in three-dimensional spiral polyester staple fiber for Special Smoothness.
It is a four component silicone oil which consists of HY-8881, HY-8882, HY-8883, and HY-8884.
HY-8881 50% special type reactive Organosilicon Emulsion
HY-8882 50% reative organosilicon Emulsion
HY-8883 15% special type Organosilicon catalyzer and fast-dryer
HY-8884 98% special type Organosilicon Cross-linking agent
Ingredient of Silicone Oil | Dosage | Standard |
HY-8881 | 60-80 | 70 |
HY-8882 | 30-10 | 20 |
HY-8883 | 10 | 10 |
HY-8884 | 1~4 | 4 |
1. Conditional of Cross-linking
Temperature(ºC) | Time(minutes) |
120 | >20 |
130 | >10 |
140 | 10 |
150 | 8 |
160 | 4 |
170 | 3 |
2. About Pretreatment
a. It does not need predry
b. The proportion of the ingredients in emulsion can be adjusted according to different fiber denier.
c. Silicone oil immitting: 0.4~0.6%.
d. Speed of Hot Air ≥ 1.5m/s
3. Method of Application
(1) Ingredient proportion in emulsion
Silicone Oil: 1 Share (HY-8881 70 shares HY-8882 20 shares HY-8883 10 shares HY-8884 4 shares)
Water : 9~18 Shares
(2) Confection ( Supposing : Water/ Silicone Oil=90kg:10.4kg , Emulsion 104kg)
a. Immit 0.4 kg HY-8884 and 90 kg water into the oil trough, then churn it slowly for about 10 minutes.
b. Immit 7 kg HY-8881 2 kg HY-8882 1 kg HY-8883 into the trough in turn , then churn it for 20 minutes.
c. Application: the confected emulsion has been ready for using in fiber handling (Impregnating in Oil Through or Sprinkling).
(3) Water percentage in fiber before Torrefaction <10%
(4) Emulsion contained: 8~10%
(5) Organosilicon contained: o.4%-ol6%
(6) Torrefaction: 140ºC ~180ºC*10 minutes
(7) Temperature in the Oven:
No.1 area of oven: 150ºC
No.2 and No.3 area of oven: 160ºC
4. Notice
a. Techniques of using oil trough: Silicone Oil should be added in time according to the fiber output.
b. Water content of the fiber after Torrefaction : <0.1%
c. Quality Valid: within twelve months, keep sealed.
d. DO NOT MIX WITH ANY ANION AUXILIARY!